Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring

Product Details
Customization: Available
After-sales Service: Installation and Maintain Instructions
Warranty: 15 Years
Still deciding? Get samples of US$ 0/Square Meter
Request Sample
Diamond Member Since 2021

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Registered Capital
30000000 RMB
Plant Area
>2000 square meters
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
  • Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Find Similar Products

Basic Info.

Style
Modern
Function
Anti-Slip, Moisture Proof, Rot Proof, Wear-Resistant, Fireproof, Waterproof, Soundproof, Anti-Static
Thickness
5mm
Lead Hardness
Soft
Pattern
Wood Grain
Color
Multi-Color
Usage
Household, Commercial
Transport Package
Box and Pallet
Specification
4mm, 5mm, 6mm, 7"*48", 9"*48", 12"*24"
Trademark
Trioflor
Origin
Shangdong
HS Code
3918109000
Production Capacity
500000sq. M/Month

Product Description

Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring·
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring

SPECIFICATION AND TECHNICAL DATA
DESCRIPTION Testing Method Unit  
Overall Thickness EN ISO 24346 mm 3.2-6.0
Thickness of Wear Layer EN ISO 24340 mm 0.1/0.2/0.3/0.5/0.7
Aperture between two planks Filler gauge mm 0.15
Straightness EN ISO 24342 mm 0.25
Squareness EN ISO 24342 mm ≤0.25
Curling after exposure to heat EN434 mm 1.0mm
(80C6h)
Dimensional stability after exposure to heat (%) EN 434 - 0.1%
(80C6h)
Peeling strength of layer EN 431 - ≥50N/5cm
Effect of castor chair EN 425 - No disturbance to the surface
Abrasion Resistance EN 660-2 - T/P
Scratch-resistant ISO 1518-1:2011 - 20N
Glossiness Gloss meter   ±2gu
UV Adhesion GBT9286 - 100%
Click tensile strength Electronic tension tester   1.5KN/m
UV Coating - - Diamond Core
Residual Indentation EN 433   0.1mm
Color Fastness/Grade EN ISO 105-B02 Degree 6
Fire Rating EN 13501-1   Bfl-S1
European Classification EN 685 - 23-31
Underfloor heating -   suitable
TO VC after 28 days ISO 16000-6 pg/m3 <10


WHAT KIND SPC WE CAN PROVIDE
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
EIR, Embossed In Register, The embossing matches the pattern of the color film ? looks and feel right, like real wood.
 
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Super sound proof, Special product structure allows you to enjoy a quieter environment.
 
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Herringbone, Change the traditional installation mode and be more beautiful.
 
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
Random, Random width, Random length, Non-repeat.


WHAT SIZE WE CAN PROVIDE
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring

WHAT THICKNESS WE CAN PROVIDE
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring

COLOR/DECOR
Spc Flooring Espc Vspc Engineerd Spc ABA Ab Vinyl Flooring
FAQ1
Q1: Do you offer free sample?

A1: Yes, free samples available.

Q2: What is your lead time?

A2: Within 15 days after we get the prepayment.

Q3: What is your payment terms?

A3: 30% deposit and 70% upon the copy of B/L.

Q4: How do I properly clean and maintain my SPC flooring?

A4: To clean dirt that won't come up with a sweep or vacuum, use a non-rinsing cleaner that
leaves no film and a mop. Never use an abrasive cleaner, oil cleaner, or dish detergent.

Q5: Can I walk on my SPC floor and mop it immediately after installation?

A5: It is not recommended that you walk on your SPC floor after installation for at least 24
hours. You can mop your floor immediately after installation.

Q6: How do I repair a chip or scratch in my vinyl flooring?

A6: Chips and deep scratches in SPC generally cannot be removed, but can be hidden or
concealed. To remove scuff marks try rubbing a drop of mineral spirits, turpentine, paint
thinner, or baby oil over the mark. Then wipe the scuff away with a soft cloth. Be sure to
wipe the SPC floor thoroughly with a damp cloth afterwards, as these solutions can leave.


 