SPECIFICATION AND TECHNICAL DATA
DESCRIPTION |
Testing Method |
Unit |
|
Overall Thickness |
EN ISO 24346 |
mm |
3.2-6.0 |
Thickness of Wear Layer |
EN ISO 24340 |
mm |
0.1/0.2/0.3/0.5/0.7 |
Aperture between two planks |
Filler gauge |
mm |
≤0.15 |
Straightness |
EN ISO 24342 |
mm |
≤0.25 |
Squareness |
EN ISO 24342 |
mm |
≤0.25 |
Curling after exposure to heat |
EN434 |
mm |
≤1.0mm (80C6h) |
Dimensional stability after exposure to heat (%) |
EN 434 |
- |
≤0.1% (80C6h) |
Peeling strength of layer |
EN 431 |
- |
≥50N/5cm |
Effect of castor chair |
EN 425 |
- |
No disturbance to the surface |
Abrasion Resistance |
EN 660-2 |
- |
T/P |
Scratch-resistant |
ISO 1518-1:2011 |
- |
≥20N |
Glossiness |
Gloss meter |
|
±2gu |
UV Adhesion |
GBT9286 |
- |
100% |
Click tensile strength |
Electronic tension tester |
|
1.5KN/m |
UV Coating |
- |
- |
Diamond Core |
Residual Indentation |
EN 433 |
|
≤0.1mm |
Color Fastness/Grade |
EN ISO 105-B02 |
Degree |
≥6 |
Fire Rating |
EN 13501-1 |
|
Bfl-S1 |
European Classification |
EN 685 |
- |
23-31 |
Underfloor heating |
- |
|
suitable |
TO VC after 28 days |
ISO 16000-6 |
pg/m3 |
<10 |
WHAT KIND SPC WE CAN PROVIDE
EIR, Embossed In Register, The embossing matches the pattern of the color film ? looks and feel right, like real wood.
Super sound proof, Special product structure allows you to enjoy a quieter environment.
Herringbone, Change the traditional installation mode and be more beautiful.
Random, Random width, Random length, Non-repeat.
WHAT SIZE WE CAN PROVIDE
WHAT THICKNESS WE CAN PROVIDE
COLOR/DECOR
FAQ1
Q1: Do you offer free sample?
A1: Yes, free samples available.
Q2: What is your lead time?
A2: Within 15 days after we get the prepayment.
Q3: What is your payment terms?
A3: 30% deposit and 70% upon the copy of B/L.
Q4: How do I properly clean and maintain my SPC flooring?
A4: To clean dirt that won't come up with a sweep or vacuum, use a non-rinsing cleaner that
leaves no film and a mop. Never use an abrasive cleaner, oil cleaner, or dish detergent.
Q5: Can I walk on my SPC floor and mop it immediately after installation?
A5: It is not recommended that you walk on your SPC floor after installation for at least 24
hours. You can mop your floor immediately after installation.
Q6: How do I repair a chip or scratch in my vinyl flooring?
A6: Chips and deep scratches in SPC generally cannot be removed, but can be hidden or
concealed. To remove scuff marks try rubbing a drop of mineral spirits, turpentine, paint
thinner, or baby oil over the mark. Then wipe the scuff away with a soft cloth. Be sure to
wipe the SPC floor thoroughly with a damp cloth afterwards, as these solutions can leave.
Waterproof Vinyl Tiles Spc flooring, 4mm/4.5mm/5.0mm with 0.3mm/0.5mm wearlayer,100%Virgin Material UV Surface Waterproof Vinyl Tiles Spc flooring, 4mm/4.5mm/5.0mm with 0.3mm/0.5mm wearlayer,100%Virgin Material UV Surface Waterproof Vinyl Tiles Spc flooring, 4mm/4.5mm/5.0mm with 0.3mm/0.5mm wearlayer,100%Virgin Material UV Surface Waterproof Vinyl Tiles Spc flooring, 4mm/4.5mm/5.0mm with 0.3mm/0.5mm wearlayer,100%Virgin Material UV Surface Waterproof Vinyl Tiles Spc flooring, 4mm/4.5mm/5.0mm with 0.3mm/0.5mm wearlayer,100%Virgin Material UV Surface